We use cookies to continually optimise our website. By continuing to use this website, you agree to the use of cookies. For more information, please see our User Conditions. OK

Images 

Back to Search

Pipelaying Process 4

The double-joint is moved to the non-destructive testing station where every millimetre of the weld undergoes ultrasonic testing to detect any unacceptable flaws. If required, the defect will be repaired and the weld rescanned to meet international quality standards